Friday, December 31, 2010

Re: [MW:9042] reason for burnthrough defect

Dear Sankar,

The following are the main reason for burn through:

1.  Very slow travel speed and high current.
2.   High heat input.
3.   Large root opening.
4.   Uneven root face.
5.   Unskilled welder or welding operator.

Thanks & Regards.
Manoj

On Thu, Dec 30, 2010 at 7:30 PM, shankark <shankark.qc@gmail.com> wrote:
we got BT defect in smaw process welding using E6010 for root, and
E7018 for hotpass, capping. what could be the reason for this defect
and how we can avoid it.

thanks,
shankar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...