Dear K.C.

The basics is that one needs to know client specifications for base material type, welding position, welding process to be used, joint configuration (single V, single bevel, J prep, compounded weld, etc....), heat input allowed.

Then, the consumable selection is taken into account because a WPS and WQ will be required (I imagine).

After running the procedure qualification, then you know what to do and how to do the job.

 

 

Regards

 

Ariel Tendeiro

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kshitish tripathy
Sent: Thursday, 30 December 2010 2:36 PM
To: materials-welding@googlegroups.com
Subject: [MW:9010] Fw: CONSUMABLE SELECTION FOR JOINT OF DIFFERENT THICKNESSES.

 



On Thu, 30 Dec 2010 12:03:09 +0530 "kshitish tripathy"kshitish.tripathy@rediffmail.com wrote
DEAR ALL,
KINDLY SUGGEST ME THAT AS PER IS CODE WHAT WILL BE THE CONSUMABLE SELECTION WHILE WELDING THE JOINT OF DIFFERENT THICKNESSES. WHETHER THE GROOVE DESIGN & CONSUMABLE SELECTION WILL BE AS PER LOWER THICKNESS ONE. IN WHICH NUMBER OF IS CODE IT IS THERE; PL. GUIDE ME.


THANKING YOU


K.C.TRIPATHY
SR.QA/QC ENGG.
UHDE INDIA LIMITED
IOCL PARADEEP SITE.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...