Hi

Consumable selection is not going to play a role in dissimilar thicknesses case, your design code may restrict you from welding if thickness difference is exceeding the code requirement. Please mention your design code, material specs and parameters, to see if there could be some metallurgical issues as well.

Regards
Manpreet Singh

 

On Thu, 30 Dec 2010 12:36:19 , "kshitish tripathy" <kshitish.tripathy@rediffmail.com> wrote


On Thu, 30 Dec 2010 12:03:09 +0530 "kshitish tripathy"kshitish.tripathy@rediffmail.com wrote
DEAR ALL,
KINDLY SUGGEST ME THAT AS PER IS CODE WHAT WILL BE THE CONSUMABLE SELECTION WHILE WELDING THE JOINT OF DIFFERENT THICKNESSES. WHETHER THE GROOVE DESIGN & CONSUMABLE SELECTION WILL BE AS PER LOWER THICKNESS ONE. IN WHICH NUMBER OF IS CODE IT IS THERE; PL. GUIDE ME.


THANKING YOU


K.C.TRIPATHY
SR.QA/QC ENGG.
UHDE INDIA LIMITED
IOCL PARADEEP SITE.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...