Dear Mr.Srinivas,

Please refer to  API 620 10th edition,2002

Chapter 5.26 and Table 5.2 will explain the RT requirements for the construction of tanks as per the above code.


Thanks and Regards,


Thiru.

Mechanical Engineer Consultant,

Angola.

--- On Wed, 29/12/10, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:

From: Srinivas Engr <srinivas.gmsrini@gmail.com>
Subject: [MW:8995] RT requirements for Tanks as per API 620?
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Wednesday, 29 December, 2010, 7:57 PM

Dear All

Could anybody pl clear wats the RT requirement for Tank with Shell
thickness of 12mm as per API 620?
Where to refer & Wat is the requirement?

Rgds
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...