Dear All,
We need to fabricate a piping with carbon steel and low
alloy steel welding electrode section i saw one project 6010 for root
alternate passes 7010.But both cellulose electrodes(high hydrogen
content)may be chances there hydrogen cracking please give ELECTRODE
QUALIFICATION TEST details(as per ASTM standard)


Regards,
Devendar G

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...