Tuesday, December 28, 2010

[MW:8967] crack

Dear member,

During welding shell to intermediate dish end buttjoint, Root pass is
completed by SMAW (shell is not rotating). Before star to fill the
joint by SAW(shell is rotating), during preheat crack is came in
between weld and shell. can we issue NCR and better ndt method?

Regards
Mani

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...