For Welder Qualification as per Section IX there is no variable for
Impact . As far as base metal is concerend the only variable is 403.16
& 403.18 in case of SMAW.
As per below extract from ASME Section IX:
QW-303.1 Groove Welds — General. Welders and welding operators who
pass the required tests for groove
welds in the test positions of table QW-461.9 shall be qualified for
the positions of groove welds and fillet welds
shown in table QW-461.9. In addition, welders and welding operators
who pass the required tests for groove welds
shall also be qualified to make fillet welds in all thicknesses and
pipe diameters of any size within the limits of the
welding variables of QW-350 or QW-360, as applicable
Best Regards,
JASPAL SINGH CWI-AWS, CSWIP-3.1
ISGEC-PED, Yamunanagar, Haryana (India) PH: +911732307251 ; Mob.
+918930111441(CUG), +919996624244
www.isgec.com
On Dec 30, 7:54 am, "manpreet " <manpreetsi...@rediffmail.com> wrote:
> Dear All,According to QW-451.4, Groove weld qualifies for all thickness ranges of fillet welds,In production a a fillet joint with 25mm & 13mm, impact test required,Is the code saying that QW-403.6 & QW-451.1 will not be applicable here? Please give me your views.....RegardsManpreet Singh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments