Re: [MW:8963] Clarrification regarding Material Inspection

Anand,

First you need to get it clarified whether it is for Upstream or for refinery. The applicable standard for upstream is NACE MR0175 and for Refinery it is NACE MR 0103.

Normally we need to check the products Heat Treatment Form and the Hardness plus the chemistry as it is specified for stainless steels.

J.GERALD JAYAKUMAR 00919344954677  


--- On Mon, 12/27/10, AnandM@punjlloyd.com <AnandM@punjlloyd.com> wrote:

> From: AnandM@punjlloyd.com <AnandM@punjlloyd.com>
> Subject: [MW:8959] Clarrification regarding Material Inspection
> To: materials-welding@googlegroups.com
> Date: Monday, December 27, 2010, 3:03 PM
>
> Dear All,
> Pls Clarify, what are the characteristics to verified for
> Sour service
> material inspection. Kindly mention any important point to
> be check.
>
> With Regards
>
> Anand.M
>
>
>
>
> ---------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------
>
>
> This e-mail and any files transmitted with it are for the
> sole use of the intended recipient(s) and may contain
> confidential and privileged information. If you are not the
> intended recipient of this communication, we request you to
> notify the sender immediately by return email and destroy
> all copies and the original message. Any unauthorized
> review, use, disclosure, dissemination, forwarding, printing
> or copying of this email is strictly prohibited. The
> recipient acknowledges that Punj Lloyd Limited or its
> subsidiaries and associated companies (collectively "Punj
> Lloyd Group") are unable to exercise control or ensure or
> guarantee the integrity of/over the contents of the
> information contained in e-mail transmissions and further
> acknowledges that any view, opinion or advice expressed in
> this message are those of the individual sender and no
> binding nature of the message shall be implied or assumed
> unless the sender does so expressly with due authority of
> Punj Lloyd  Group. Although we have taken all
> reasonable precautions to ensure that this communication is
> free from viruses. We do not assume responsibility for any
> loss or damage arising from the use of this email.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...