Thursday, December 30, 2010

[MW:9025] Technical solution

Dear All,

When we use GTAW , we are using  ER-70S2/E-7018( Same tensile) combination, alternatively in SMAW , we are using E-6010/E-7018( Different tensile) instead of E-7010. E-7010 is not available(as per ASME) in the market. Is there any technical problem to manufacture it or to  use it.

Can somebody tell it.

Regards

Pradip

--