Tuesday, December 28, 2010

Re: [MW:8968] crack

Mani,

Please let us know the materials involved (Shell & dished end), joint configuration, thickness and the welding consumables used to weld the joint.

Also please let us know the crack orientation, was it longitudinal or transverse to the weld axis.

Whether preheat was maintained after completion of SMAW pass?

Regards,

Praveen


--- On Tue, 12/28/10, Mani <kumarmani12@gmail.com> wrote:

> From: Mani <kumarmani12@gmail.com>
> Subject: [MW:8967] crack
> To: "materials-welding" <materials-welding@googlegroups.com>
> Date: Tuesday, December 28, 2010, 1:17 PM
> Dear member,
>
> During welding shell to intermediate dish end buttjoint,
> Root pass is
> completed by SMAW (shell is not rotating). Before star to
> fill the
> joint by SAW(shell is rotating), during preheat crack is
> came in
> between weld and shell. can we issue NCR and better ndt
> method?
>
> Regards
> Mani
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members
> personel views and meant for educational purposes only,
> Users must take their own decisions w.r.t. applicable
> code/standard/contract documents.
>


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...