Re: [MW:6804] P91_SR

Dear Ravindra
Use capacitor discharge unit to attach TC to job to measure metal temp
Regards
Hegde

Sent from my BlackBerry® smartphone from !DEA


From: "Ravinder Sharma" <ravinder@isgec.com>
Sender: materials-welding@googlegroups.com
Date: Mon, 30 Aug 2010 18:05:49 +0530
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:6786] P91_SR

 

 

Hi friends ,

Can anybody suggest better way to attach thermocouple on P91 pipe for SR avoiding the welding, in non- calibrated furnace? Metal temperature to be measured directly.

 

Ravinder Sharma