Thursday, August 26, 2010

[MW:6716] Charpy Test

Hi There,

 

We have an existing WPS, The existing WPS doesn’t have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.

 

 

Thank you,

 

Larry Zarate

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...