Hi,
Yes you can, provided the maximum deposit of weld metal within limit given in QW 451.1. Refer QW 200.2 (f) for multiple WPS from single PQR.
Regards,
Ibrahim
On 5 March 2010 03:54, SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in> wrote:
Dear All,I have qualify the PQR using proposed wps Process are GTAW/SMAW/SAW.After all NDT & DT completed on same and actual WPS prepared and production weld also done using that WPS with same welding process.Now my production dept want to rewrite the WPS using only GTAW & SAW due to repairs on production welds. Because repairs are @ SMAW weld location.QW-200.4 is permitting this?Thank you,Regards,S.Senthilkumar
The INTERNET now has a personality. YOURS! See your Yahoo! Homepage. --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Regards
Muhammed Ibrahim PK
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment