Friday, March 5, 2010

Re: [MW:4441] RE: 4425] Procedure qualification Record (PQR)

Under the condition that you have recorded those thicknesses


  From: "Bathula Raghuram (Mumbai - PIPING)" [R.Bathula@ticb.com]
  Sent: 05/03/2010 09:33 ZE5B
  To: <materials-welding@googlegroups.com>
  Subject: [MW:4426] RE: 4425] Procedure qualification Record (PQR)


you can, however consider weld metal thickness (t) qualified for individual process as per QW451.1


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of SENTHILKUMAR SWAMINATHAN
Sent: Friday, March 05, 2010 9:25 AM
To: Engineering
Subject: [MW:4425] Procedure qualification Record (PQR)

Dear All,
 
I have qualify the PQR using proposed wps Process are GTAW/SMAW/SAW.
After all NDT & DT completed on same and actual WPS prepared and production weld also done using that WPS with same welding process.
 
Now my production dept want to rewrite the WPS using only GTAW & SAW due to repairs on production welds. Because repairs are @ SMAW weld location.
 
QW-200.4 is permitting this?
 
Thank you,
Regards,
S.Senthilkumar


 

1 comment:

Anonymous said...

Amiable brief and this post helped me alot in my college assignement. Thanks you as your information.

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...