Depending on application:
Lincoln Electric 780 flux
Lincoln Electric P223 flux
Lincoln Electric 781 flux
Lincoln Electric SPX 80
Etc.
From: "GERING, Erwin" [Erwin.GERING@airliquide.com]
Sent: 03/05/2010 08:48 AM CET
To: <materials-welding@googlegroups.com>
Subject: [MW:4435] RE: 4421] Hispeed fluxes for SAW WELDING
Depending on application:
Oerlikon OP F55
Oerlikon Uniflux D1
Oerlikon OP 191
Etc…
With kind regards,
Erwin GERING
Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens bcube bcube
Verzonden: donderdag 4 maart 2010 16:39
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:4421] Hispeed fluxes for SAW WELDING
Dear all,
Can any one sent me the details releated to the Hi speed fluxes used for SAW welding .
Reg,
RBG
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment