Thursday, March 4, 2010

Re: [MW:4413] evaluating based on AWS D1.1 for UT

Refer Annexure (No I forgot) it says alternative method you can use DAC.
S.Senthilkumar

--- On Wed, 3/3/10, Ali Asghari <asghariali@rocketmail.com> wrote:

From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:4407] evaluating based on AWS D1.1 for UT
To: materials-welding@googlegroups.com
Date: Wednesday, 3 March, 2010, 5:35 PM

Dear All
what is the sensitivity refrence line for ultrasonic testing according AWS D1.1?
is DAC applicable?(if yes, in which paragraph this refered?)
regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...