thickness) it is necessary to qualify separate PQR for with PWHT or
without PWHT.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Kamalaksha,
Arekere
Sent: Thursday, March 04, 2010 9:00 AM
To: materials-welding@googlegroups.com
Subject: [MW:4412] WPS
Dear all ,
If we qualify the welding procedure for the P1 materials with post weld
heat treatment then whether it is applicable for the welding without
post weld heat treatment , Please note that here thickness is not the
criteria .Post weld heat treatment is required for some of the process
line in Refinery.
Please clarify.
Kamalaksh. A
GLIS GmbH -India
Mobile: +919741506305
Email : kare@gl-group.com
Website: www.gl-group.com
Filtered by Hosted Filtering
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments
can anyone clarify whether PWHT is a code requirement or design requirement, because I have seen requirement of PWHT only in some codes like ASME B31.3 and 31.4 based on pipe thickness.
What is the actual criteria for including PWHT in a WPS.
Regards
Harikrishnan N S
QA/QC Engr
Punj Lloyd Ltd.
However PWHT also required due to process reasons, when corrosive fluids are involved, like Wet H2S, H2, Caustic, Amine etc. which is to defined by process designer based on operating conditions.