Re: [MW:3969] welding procedure for the material at - 30degree C

Check the welding consumable(s), whether can satisfy the ASME Sec-II part-C requirement at -30 deg C,
then perform another PQR following all the variables identical to the previous on and only perform the impact testing at -30 deg C.
 
Regards,

On Tue, Jan 5, 2010 at 3:02 PM, John Manoj <manojacgnr@gmail.com> wrote:
In my oppinion you can use the same procedure but you have to do only impact test at -30 degree C with the same parameters. You no need to repeat all other mechanical tests.

Regards.
Manoj John

 

On Tue, Jan 5, 2010 at 8:57 AM, Elshan Feyzullayev <elshan_f@hotmail.com> wrote:
Dear Friends,
 
I have a welding to do on the material where the service temperature is -30 degree C. I have got a welding procedure which charpy V test was carried out at -20 degree C. can I use this procedure for welding of the material which the service temperature is -30 degree C?
 
regards,
Elilk.


Windows Live: Make it easier for your friends to see what you're up to on Facebook.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Sukamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...