Right now I do not have the EIL spec no but I do have MECON Ltd's spec no which is exactly in line with EIL spec.Mecon std no is "MEC/SD/05/62/06/01"
Regards
Aarpee

On Wed, Oct 21, 2009 at 1:36 PM, PRAVEEN KUMAR <praveenkumar.sek@gmail.com> wrote:
Dear aarpee,
Thanks for ur info.
pls give me ASME stds  & EIL specifi.No
 
 
Regards,
Praveen


On Wed, Oct 21, 2009 at 11:58 AM, Ramprasad Chari <ramprasad.chari@gmail.com> wrote:
+/- 3mm on spool lengths and attachments
+/- 1.5mm lateral translation
+/- 1.5mm rotational
+/- 1.0 mm out of alignment
Above is as per Engineers India Ltd specs
Regards
Aarpee

On Wed, Oct 21, 2009 at 11:08 AM, Sadique Sheikh <sadiq.mech@gmail.com> wrote:

Good morning to all group member.
I would like to as that how much deviation is acceptable in pipe
alignment for plumb and levelness?
Can we confirm alignment with level guage only or it has some
tolerences from codes?
Plz give me detail with references.
Thanks in advance.
Regards
Sadique --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...