Tuesday, October 13, 2009

[MW:3500] Re: Welding of Sa-335 to SA-106

Dear jimmy,
 
According to ASME sec IX ,
 
If you have PQR for any metal having P.No 4 to P.No 4 , you can weld any metal having P.No 4, 3 and P.No 1
 
Regards,
 
Mubarak.

 
 

 
On 10/12/09, Jimmy Nielsen <nielsen.jimmy@gmail.com> wrote:

Hello Gents

Can sombody help me with a answar regarding welding of Sa-335 to
SA-106.

I have a PQR covering material 335-P11 to 335-P11( P4)
Can I use it for welding of P-no 4 to P-no 1

Regard, jimmy




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...