Tuesday, October 13, 2009

[MW:3499] Re: Welding of Sa-335 to SA-106

Jimmy,
 
ASME Sec-IX allows a PQR qualified for P4-P4 base metal to be referred as the supporting PQR for a WPS on P4-P1 base metal.
You need to ensure, that the design code calls for the only ASME Sec--IX, for welding qualifications,welding comsumables are same as in the PQR,there are no other rquirements, such as clients' spec etc.
 
I do not have the applicable clause handy,but if you need more details I may send the info to you.
 
Thanks
 
Pradip Goswami
Welding Engineer/Specialist
Ontario Power Generation Inc.
Tel-1-519-5872201,Ext3107
 
 

 
> Date: Mon, 12 Oct 2009 01:50:08 -0700
> Subject: [MW:3490] Welding of Sa-335 to SA-106
> From: nielsen.jimmy@gmail.com
> To: materials-welding@googlegroups.com
>
>
> Hello Gents
>
> Can sombody help me with a answar regarding welding of Sa-335 to
> SA-106.
>
> I have a PQR covering material 335-P11 to 335-P11( P4)
> Can I use it for welding of P-no 4 to P-no 1
>
> Regard, jimmy
>
> --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...