Hi,

 

As per QW-424, you can support P4 to P4 PQR for P4 to P1. However, the below are needs to be consider for its requirement.

 

1. Check for PWHT with time &temperature requirement. If any

2. Impact Requirement for SA 106 ( HAZ). If any

 

Regards,

Vasanth

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jimmy Nielsen
Sent: 12 October 2009 09:50
To: Materials & Welding
Subject: [MW:3490] Welding of Sa-335 to SA-106

 

 

Hello Gents

 

Can sombody help me with a answar regarding welding of Sa-335 to

SA-106.

 

I have a PQR covering material 335-P11 to 335-P11( P4)

Can I use it for welding of P-no 4 to P-no 1

 

Regard, jimmy

 

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...