Monday, October 12, 2009

[MW:3488] RE: 3482] Re: WPS/PQR, Range Qualified

Hi,
 
There is no restriction on thickness or diameter for the PQR. It is requireq for the performance (WPQT) only.
 
Regards,
 
R.Gopalasamy,
Sr.QA/QC Consultant,
Hindustan Oil Exploration Company Ltd,
PY1, Onshore Gas Processing Facility,
Thirukkadaiyur.
email : rgopalasamy @hoec.com
Mobile : 09789090752


-------------------------------------------------------------------- HOEC Email Disclaimer : http://www.hoec.com/email_disclaimer.htm



From: materials-welding@googlegroups.com on behalf of PREM SHANKARDUTT NAUTIYAL
Sent: Sun 10/11/2009 7:24 PM
To: raghurambathula@gmail.com
Cc: materials-welding@googlegroups.com
Subject: [MW:3482] Re: WPS/PQR, Range Qualified

Hi

What i interpret from the query is that the thickness of test coupon welded for PQR i.e while qualifying the WPS was 15mm.

Hence as per ASME SecIX, QW-451:which states the Procedure qualification thickness limits, the range of thickness "T" of base metal qualified will be 5mm to 30mm (2T).

Actually the question is not very clear and imp. details like impact requirements are missing ..

All are requested to pose clear,detailed to the point queries so that they can get correct answers / solutions.

Regards

Prem Nautiyal
Cell:9820313278

On Sun, 11 Oct 2009 14:06:21 +0530 wrote
>thickness limits are defined in QW 403.6 and 403.8, diameter is not a restriction for procedure but thickness limits are.to weld  20mm thickness your PQR test coupon thickness shall be at least 10mm
On Sun, Oct 11, 2009 at 10:53 AM, Shashank Vagal wrote:
Hi Group Members,Please see the following and advise.Shashank Vagal

Query:

dear every one,

i have this problem i need to know the thickness range or pipes diameter
range for the wps in which standard i think its in asme sec 9 but where ???

for exmple if i have wps for thickness 15 is it cover the 20 mm

waiting answer please

regards

My Reply:

 

A WPS is a guideline to ensure joint integrity as proven by
PQR + applicable mech tests + NDT. It is intended for all job sizes once the
welding technique used proves itself in these tests. The sizes etc come in to
picture by qualifying welder on test coupons of a given size as per your job
requirements. ASME IX stipulates weld metal deposit and not job size. Please
ref to QW 450 - 461.


Now, send attachments up to 25MB with Yahoo! India Mail. Learn how






PREM S NAUTIYAL
CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---