Hi ,
P no is assigned to all materials under ASME SEC IIA and IIB.
S no is asigned to materials that are permitted to use by ASME B31 code for pressure piping.
Note that material qualified having certain P no qualifies corresponding S no however viceversa is not true
Regards
Sachin

On Sun, 11 Oct 2009 13:59:06 +0530 wrote
>Hi Friends
>

>
As per ASME Sec.IX, QW420, materials are grouped and assigned P-Numbers i.e. Parent material number.
>

>
Similarly i would like to know what is meant by S-Number with full form and detailed explanation !!!
>

>

>
Regards
>

>
Prem NautiyalPREM S NAUTIYAL
>
CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---