dear every one,

i have this problem i need to know the thickness range or pipes diameter range for the wps in which standard i think its in asme sec 9 but where ???

for exmple if i have wps for thickness 15 is it cover the 20 mm

waiting answer please

regards


My Reply:

 

A WPS is a guideline to ensure joint integrity as proven by PQR + applicable mech tests + NDT. It is intended for all job sizes once the welding technique used proves itself in these tests. The sizes etc come in to picture by qualifying welder on test coupons of a given size as per your job requirements. ASME IX stipulates weld metal deposit and not job size. Please ref to QW 450 - 461.




Now, send attachments up to 25MB with Yahoo! India Mail. Learn how
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...