Hi Nimesh

Use TIG process and filler wire:ER316, dia.1.2mm OR 1.6mm.
If you use ER316L, much better.

Regards

Prem Nautiyal
Cell:9820313278

On Fri, 09 Oct 2009 15:08:17 +0530 wrote
>
Dear All,



Kindly suggest which method to use for welding SS304 Tube sheet (6mm)
to SS316 Tube (25mm). It is for a chiller to operate at -40 Degrees C.
The pressure is only 2 bar. Also what consumable to use for filler
material / for MMA welding



Regards,



Nimesh S Chinoy









31, Mistry Industrial Complex,

Cross Road 'A', M.I.D.C.

Andheri(East), Mumbai -93



www.electronicsdevices.com

Tel :+91-22-26870313 / 318

Fax: +91-22-26874629




--
Nimesh S Chinoy




PREM S NAUTIYAL
CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...

Pages

Contributors

Blog Archive