Dear all,

I have a vessel SS 347 clad on P4 material. The vessel is to be used
in H2s service at a temperature of 530 deg C. Specification is asking
for autoclave/ H2 disbonding test for weld overlay. what are the
basis to decide for the test? Is it neccessary to do at 530 deg C or
there is any other permutation or combination to do the test at lesser
temp?

If yes please guide
regards,
Amarjit singh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...