Dear Ali,
Answer to your query...
----------------------------
is it correct that for steels that has a specification another of
asme
II find equivalent steel,P no ?
---------------------------------
Metals that do not appear in ASME Sec IX - P Number Table are
considered to be unassigned metals; the unassigned metal can be
matched with ASME P Number of the table by UNS Number of unassigned
metal. The metals do not having UNS numbers which are not listed in P
Number table can be matched by Chemical & Mechanical properties (UTS)
of the materials that are available in Section II by a comparison
table. Hence, it is correct that a spec of Non ASME material can be
compared with ASME P Numbering system.

Thanks
Senthil


On Aug 27, 8:19 am, ali asghari <asgharial...@gmail.com> wrote:
> Dear all
> is it correct that for steels that has a specification another of asme
> II find equivalent steel,P no ?
> regards.
>
>
>
> On Wed, Aug 26, 2009 at 9:26 AM, Muhammad Ijaz <m_i...@ffc.com.pk> wrote:
> >  Dear Mano,
>
> > As per Stahlschluseel 2007, G4859 is equivalent to A351 (CT15C). So the
> > corresponding P no. shall be P. no. 45 as per ASME IX 2007.
>
> > Regards,
>
> > *Muhammad Ijaz*
>
> >  ------------------------------
>
> > *From:* materials-welding@googlegroups.com [mailto:
> > materials-welding@googlegroups.com] *On Behalf Of *Manoharan Kalimuthu
> > *Sent:* Tuesday, August 25, 2009 9:56 PM
> > *To:* materials-welding@googlegroups.com
> > *Subject:* [MW:3018] p no
>
> > Dear all
>
> > We have material G4859 (its in the ISO) I would like to know what is the P
> > NO for this ....
>
> > Regards
>
> > Mano- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...