> REPLY
>
> Dear Member/s,
>
> THe quickest method is to fist  calculate volume of  the V- groove .
> Multiply this volume with density to get theoreticall weight of weld
> metal. Now we know that the actual weight used is much more than the
> theoretical weight since there are butt losses,electrode coating has
> to be accounted for and there is convexity at the top and  root of
> joint.
> Thus the  weld metal weight therefore =theoretical weight xQ factor
> ( Quantity  factor) .This Q factor=2 for TIG welding and 2.5 for SMAW.
>
> Hope this thumb rule will help you calculate weight of  welding
> electrode/wire required for a joint..
>
> Sorry that for your second query for gas consumption I am unable to
> respond.
>
> Chander Girotra
> ==========================================================================================================================
>
> On Aug 25, 2:48 pm, Sujeet Sangle <sujeetsan...@gmail.com> wrote:
>> Dear Memebers ,
>>
>> I need to calculate quantity for SMAW consumable  for Structural Electrodes
>> for V Groove different thickness and Diameter
>>
>> TIG consumable for piping work different thickness and Diameter .
>>
>> Together with the Pre heating gas consumption .
>>
>> Can any one guide me for the above .
>>
>> Thanks
>>
>> Sujeet
>
> >
>

--
Daniel Iordache
Bureau Veritas - Angola
Mechanical Surveyor
Mobile Ao: +244921544583
Mobile Ro: +40721731728
E-Mail: daniel.iordache@gmail.com
daniel_iordache@yahoo.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...