Change in P Number is an essential variable, P1 to P1 and P8 to P8
can't be welded with the WPS qualified; but P1 to P8 can be welded

Thanks
Senthil

On Aug 24, 8:57 am, Kural <kura...@gmail.com> wrote:
> Interpretation: Answer is yes ( for all 3 combination of basemetals) as long
> as other essential and supplemtary essential are unchanged.
>
> On Sun, Aug 23, 2009 at 9:48 PM, Sukamal Naskar <sukamalbec...@gmail.com>wrote:
>
>
>
> > Dear All,
> > Good Morning !!!
>
> > I have a query on ASME SEC-IX ( 2007 ED, 08 ADD )
>
> > QW-403.5 (c ) , states that " ---------------   In addition, when base
> > metals of two different P-Number Group Number combinations are qualified
> > using a single test coupon, that coupon qualifies the welding of those two
> > P-Number Group Numbers to themselves as well as to each other using the
> > variables qualified."
>
> > *Query: If we qualify one PQR, with P-No. 1 Gr. No 2  to  P-No.8 Gr.No.1
> > material using  SMAW ( E 309MoL) process with impact testing  on weld metal
> > & both HAZ portion , does this PQR supports the following WPS combination of
> > base metals , if all other welding variables are unchanged ?*
>
> > * *
>
> > *(i)                  **P-No. 1 Gr.No.2  to  P-No. 1 Gr.No.2  *
>
> > *(ii)                **P-No. 1 Gr.No.2  to  P-No. 8 Gr.No.1  *
>
> > *(iii)               **P-No. 8 Gr.No.1  to  P-No. 8 Gr.No.1  *
>
> > Please give your comments,
>
> > Thanking you,
> > Regards,
> > --
> > Sukamal Naskar
> > Malaysia- Hide quoted text -
>
> - Show quoted text -

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...