Yes, we use 3M strip plastic brush. There are several grades it depend of the job conditions.

fg

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Amarjit Singh
Sent: sábado, 22 de Agosto de 2009 8:20
To: Materials & Welding
Subject: [MW:2986] Monel N4400


Dear all,

Is there any process( Mech or chemical) for cleaning of Monel N4400
after welding & overlay. If yes which process is suitable mechanical
or chemical. Please provide any suitable reference

regards,
amarjit singh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...