Dear Javed, Enclosed the details,Regards,
Nom. Fig.Size
Ins. (mm)
Bolting
No. x Dia.
Ins.
Rec.
Bolt Stress
lb/in2
Torque lbf.ft. (Nm)
Bolt Lubricant
Molykote 1000 (µ = 0.11)
36 (900)
20 x 3 ½" UN8
45,000
15983
(21670)
On 8/2/09, Mohammad Javeed <mmubasharjaveed@gmail.com> wrote:Dear all
Have a nice day
I need your help about one query regarding torque value. We have a one flange joint of dia 36" RF CL. 900 material A350-LF2.and bolt length is 800mm. As per our client requirement this tightening should be done with hydraulic tensioning system. So what should be the torque value for this flange?
Thanks
M javed
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
1 comment:
Hello Mohammed,
Your query is a "mechanical oxymoron"! If you are being told that bolt tensioners must be used, your torque value question is moot: there is no torque involved when bolt tensioners are used! You might wish to see the link for further details. If you know what the required bolt stress is, you simply multiply that by the area of the bolt tensioner and then by the LoadTransferFactor (determined by the bolt dia and grip length). This will provide you with the bolt tensioner operating pressure - if you'll be tensioning 100% of the flange's bolt population simultaneoulsy. If you'll only be performing 50% tensioning, you'll have to calculate both A and B pressures.
Here's the link: http://www.heviitech.com/Hevii_Tensioner_Intro.html
Best regards,
Jörg
Post a Comment