Dear All,
Regarding above mentioned subject, i would like to know in detail about ferrite number. I have a few questions to ask such as What is the ferrite number? Why it is so important? Materials subjected to ferrite number? Permissible limit of ferrite number? Code and standard that we refer to requirement of ferrite number? Procedure to perform ferrite number?..If anybody have experience or information regarding this subject hopefully you can share with me. Thank in advance for your kind cooperation
Regards
tong2
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Re: [MW:35289] Welding consumable for S355J2WP material
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...