Sunday, July 19, 2009

[MW:2716] PWHT-Reg.

Dear friends,
Any body can help to me
 
P5B Gr2 (SA 213 T91) Dia.32X4 PWHT Required or not required. as per ASME SEX I PW 39(Thick Limit Not Given) 

 


Thanks & Regards,

K.GANESAN
Quality Control
ISGEC / ISGEC John Thompson,
A-4 Sector-24 Noida-201301 (UP)
Tel. +91-120-2411175
Direct Tel. +91-120-2411175
Mobile : +91-9952166894


Love Cricket? Check out live scores, photos, video highlights and more. Click here
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...