----- Forwarded Message ----
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, May 4, 2009 3:01:00 PM
Subject: Fw: repair qualification
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, May 4, 2009 3:01:00 PM
Subject: Fw: repair qualification
----- Forwarded Message ----
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, May 4, 2009 1:53:37 PM
Subject: repair qualification
From: Ali Asghari <asghariali@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, May 4, 2009 1:53:37 PM
Subject: repair qualification
hi
i shall run a repair welding qualification according to DNV F101(one for throught thickness,one for partial thickness).now contractor ask that two qualification are done in a one test sample in different location.
how specify locations for sampling ?(in this standard it's a figure for sampling in appendix c for qualification original weld, that attached )
if anybody have detailed information,i will be grateful for sharing it.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
No comments:
Post a Comment