A welded joint, after performing the post weld heat treatment. main purpose of PWHT is to remove the resudial stresses generated during welding. PWHT temperature, time, heating rate, cooling rate depends on the material grade, nominal thickness also service condition, following the rules of code of construction. If the welded joint require PWHT, then the applicable welding procedure should also qualified with PWHT. after PWHT the mechanical properties and also the microstructure changes with respect to  as welded condition. the tensile & hardness values decreases but impact values increases.
 
Regards 

 
On 3/2/09, pubudu weerasekara <pubudu.weerasekara@gmail.com> wrote:
did u know what is the meaning of PWHT Condition can u explain it
if u feel free just send me mail
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...