if you look for for a thumb rule about haz that it is used in each situation ,it not exist.
but i prefer some following below,considered:
chemical analysis of parent metal(carbon equivalent)
thickness of parent
H.I & preheat depends on process
joint design
if you express a special case,i can help more detail
bye


From: shailesh dave <snd2988@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Saturday, October 25, 2008 12:44:10 PM
Subject: [MW:1244] HAZ

DEAR MEMBERS,
 
WOULD YOU PLEASE TELL ME WHAT COULD ME THE THUMB RULE FOR HEAT AFFECTD ZONE DURING WELDING.
 
REGARDS,
 
S.N.DAVE
I/C QA/QC DAS ISLAND UAE





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...