A 105 is an ASTM specification dealing with forged carbon steel piping components. The steel alloy involved is a low carbon, manganese and silicon containing steel similar to AISI 1330, but with lower manganese content. 
Applications:It covers carbon steel forgings for piping applications such as flanges and fittings.

ASTM A105 - Grade II is a forging, but this grade does not appear in current standards - it is simply listed as ASTM A105 in current standards. The Grade II designation was dropped sometime after 1972. I can't tell you the exact year, since I do not have access to all of the old ASTM standards.

Regards

Prem Nautiyal
Godrej, Mumbai




On Mon, 20 Oct 2008 Ahmed Eissa wrote :
>dear ,sir
>
>what is the difference between A105 and A105 GR II  ?
>thanks
>
>__________________________________________________
>Do You Yahoo!?
>Tired of spam?  Yahoo! Mail has the best spam protection around
>http://mail.yahoo.com
>>

PREM S NAUTIYAL
CELL : 9820313278


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...