Indirectly your welder is welding SMAW on the job with backing only.Your procedure is acceptable as per Sec.IX.

Regards

Prem Nautiyal
Godrej,Mumbai

On Sat, 18 Oct 2008 Hardik Desai wrote :
>Dear sirs,
>
>One welder is qualified with Backing for SMAW process.
>One welder is doing welding for Single V Butt Joint with 2-3 gap.
>backgouging is applicable. After SMAW three run, Other run by other welder
>with FCAW process. After Backgouging Other side welding by FCAW process.
>Now my question is First welder is done SMAW with 2-3 gap without backing it
>is acceptable or not?
>I hope for your reply.
>
>Thanks & Regards
>
>>

PREM S NAUTIYAL
CELL : 9820313278


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...