Monday, October 20, 2008

[MW:1231] A105 GrII

Gr II is covered in A266, and not in A105
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com]On Behalf Of Ahmed Eissa
Sent: Monday, October 20, 2008 1:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:1228] material question

dear ,sir
 
what is the difference between A105 and A105 GR II  ?
thanks



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/