Dear sirs,
 
One welder is qualified with Backing for SMAW process.
One welder is doing welding for Single V Butt Joint with 2-3 gap. backgouging is applicable. After SMAW three run, Other run by other welder with FCAW process. After Backgouging Other side welding by FCAW process.
Now my question is First welder is done SMAW with 2-3 gap without backing it is acceptable or not?
I hope for your reply.
 
Thanks & Regards

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Unknown said...

If the qualification is based upon ASME Sec IX, as per QW 402.4 elimination of any type of Backing constitute an essential variable. Addition does not not considered as Essential variable for performance Qualification. Welder is qualified in your case.
If the qualification based upon API 1104, This constitutes an essential variable (Joint design 5.2.2(g). Addition or deletion of backing needs a new qualification. The welder is not qualified. But this interpretation is debatable.

[MW:35692]