Dear Group,

 

I need help to find out how to reduce the exposure time for heavy wall thickness RT (above 4" thickness and ID of vessels 4 meter) .

 

Composite film is one of the option. Any other idea ?

 

I heard from my client that there are accelerators available which can be used for developing the film to compensate the reduce time of exposure.

 

We are using Co-60.

 

Regards.

CK


***DISCLAIMER NOTICE ***
"This e-mail and any files transmitted with it is confidential and is intended only for the use of the recepient(s) named above.
If you are not the intended recipient, any review, retransmission, dissemination, distribution, printing, copying or use the information contained in this message or any part thereof in other manner is strictly prohibited.
If you receive this e-mail in error, please notify the sender immediately by return e-mail and delete the e-mail and any of its attachments.
Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group."

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...