the detail shown is not applicable to examine butt welded type weld.
for your info.
regards,
tagore
On Tue, Oct 7, 2008 at 9:23 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
-----Original Message-----
From: PEMMARAJU RAGHAVENDRA [mailto:rpe@hzw.ltindia.com]
Sent: Tuesday, October 07, 2008 5:30 AM
To: Bathula Raghuram (Mumbai - PIPING); skumarswami@yahoo.co.in
Subject: Re: [MW:1177] Radiography of tube to tubesheet welds
We have done extensive RT of such joints in the past.
We have adopted the back radiation technique in which the source shall be moving from the front side of the joint. We have used the roli camera without guide tube and only the cranking unit wire coupled with source pigtail shall be used.The film used was of AGFA D4 with a special type of cassette with a hole at the centre.Vide this hole on the film cassette, the source enters into its position in case of back radiation technique.
It is preferred to use low curie source of Ir-192 of the order 3 to 4Ci.
Refer the attached word file for the source and film setup.
Instead of Gamma rays, you may use micro-focus X ray machine with hooded anode target which was developed by Sasol.
regards,
RPE
Larsen & Toubro Limited
www.larsentoubro.com
This Email may contain confidential or privileged information for the intended recipient (s) If you are not the intended recipient, please do not use or disseminate the information, notify the sender and delete it from your system.
From: Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com>
Subject: [MW:1177] Radiography of tube to tubesheet welds
To: "Materials-Welding (E-mail)" <materials-welding@googlegroups.com>
Date: Wednesday, 1 October, 2008, 1:48 PM
Can anybody has experience with performance of RT on tube to tubesheet welds,
please share details for both techniques (i.e. back radiation and forward
radiation), equipment literature if any for this type RT.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments