Re: [MW:16491] Thick Aluminum Welding

It can't be welded as a single joint. You can weld with adding 10mm plates. FCAW will be the best suited and fast process.
Regards,
 
Johnson Prabu
From: Darcy <morind@bantrel.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Friday, 11 January 2013 8:04 PM
Subject: [MW:16485] Thick Aluminum Welding

I have Aluminum plate sections to be welded for a power station
busbar.  The plate is 200 mm wide, 150 mm thick in the vertical 3F
position.  There are over 100 joints to be welded.  GMAW and GTAW may
be out of the question due to the sheer volume of weld metal required
for each joint.  Please offer time saving suggestions.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...