Re: [MW:12198] DSS spools 6" sch 40 x 2mtr.lg.hydro test

prashant,

the test shall be carried till acceptance and certification without any ambiguities. refer following highlighted line

RECTIFICATION OF DAMAGE/DEFECTS

(A) Damage and/or defects detected during pre-cleaning, filling, gauging and pressure test operations shall be located and repaired or replaced by the Contractor in accordance with the pipeline construction specification. The proposed repair and/or replacement procedure shall be verified by the Contractor and approved by the Company when the actual site conditions are known.

Following the completion of repairs, the activity which has been interrupted for the repair works should be repeated in accordance with all requirements of standards until the failed activity has been successfully completed.

The Contractor shall keep complete records of all damages/defects identified and repairs that are carried out. The records shall include, but not be limited to, the following details:

a)   exact date/time, location, types and causes of the defects and/or failures

b)   method of repair used

c)   equipment, materials and personnel used.

These records shall be submitted to the Company as part of the final hydrostatic test report as specified.

(A) All defective materials such as pipes, fittings and valves which have failed during the pressure testing and have been replaced, shall be marked/labelled. The mark/label shall clearly state the location, where it came from and the cause of failure. Such material shall be held by the Contractor until the means of disposal has been agreed by the Company and as per reconciliation terms of contract.


Chandrakant Mohikar (ex. CSR- PDO SHELL, VELOSI Oman)


On Thu, Aug 11, 2011 at 12:15 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
I' ve inspected DSS spools 6" sch 40 x 2mtr.lg.hydro test at a press. of 230 kg. Test failed two times.
Pl. guide me-- How many times I can do the hydro testing of such a spool?
If there is no limit, what should be the time interval between two tests?
Thanx & Regds,
psp 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...