Re: [MW:12194] DSS spools 6" sch 40 x 2mtr.lg.hydro test

Dear Prasanth ,
 
You are a Inspector ,not from Construction person ...As far my concerns there is no limit go  for re hydro's ..but it is not general practice in construction field ....
 
Once you rejected the test then you should guide/advice to construction to meet the our requirements ..and also hence they do not have much knowledge about hydro in field ...you need to tell them to do how it will be works out......
 
Insperctor should not be a barrier for constrction ....Inspector has to inspect the test, make a report and give the proper guidence to them If work  is not met the requirements ......
 
You are not mentioned why you  rejected the test ..there is so many criteria claim to  fail the test ....so please evaluate the problem and go for next step ....
 
Thanks
 
Suresh
 


 
On Thu, Aug 11, 2011 at 4:45 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
I' ve inspected DSS spools 6" sch 40 x 2mtr.lg.hydro test at a press. of 230 kg. Test failed two times.
Pl. guide me-- How many times I can do the hydro testing of such a spool?
If there is no limit, what should be the time interval between two tests?
Thanx & Regds,
psp 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...