Dear All,
I' ve inspected DSS spools 6" sch 40 x 2mtr.lg.hydro test at a press. of 230 kg. Test failed two times.
Pl. guide me-- How many times I can do the hydro testing of such a spool?
If there is no limit, what should be the time interval between two tests?