It depends on the Flange standard you are following. For e.g. refer ASME
B16.5, para 7.8 for tolerance on the mismatch of the drilled holes/BCD. For
other standards, you may have to refer to the appropriate standards,
referred therein.
Best regards,
Prasad
mick nest
<crc1199@hotmail.
com> To
Sent by: <materials-welding@googlegroups.com
materials-welding >
@googlegroups.com cc
Subject
07/03/09 07:11 AM [MW:1714] Tolerance of flange joint
Please respond to
materials-welding
@googlegroups.com
Dear All.
Please let me know what is the tolerance ( misalignment ) for two flanges
joint together by stud bolts as per any standard.
Regards,
Mick
Windows Live™: Keep your life in sync. Check it out.
Save a tree...please don't print this e-mail unless you really need to.
Save a tree...please don't print this e-mail unless you really need to.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
[MW:34916] Applicability of Impact requirement as per ASME B31.3
Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material to be used used during Fabrication - SA 333Gr6 (P No.1 G...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment