Depends on Design code and applicable impact test requirements else you can use X46 to X46 pqr



On Mon, 16 Jan 2023 at 8:56, Karunakaran Karan
<karunaqc@gmail.com> wrote:
Hi experts,
   for perform PQR  on material API 5L X46 and X70 need separate PQR, X46-P1GR1  and X70 -P1 GR-3
                
   Thanks and regards,

     S.KARUNAKARAN,
      karunaqc@gmail.com
      91-6382279754
      91-7826930029(Whats app).







On Mon, Jan 16, 2023 at 11:09 AM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Some snapshot from sec ViiiDiv.I for reference.

Inline image

Inline image

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 03:38:36 pm GMT+3, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Just to add. Charpy Impact test at MDMT (Minimum design Metal temperature) but if you perform at -48degC it can be used in the future.

API 5L X60 if ordered with special impact test requirement at -48degC then it will meet the requirement.

See below snap shot below.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 03:32:24 pm GMT+3, Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:


 thanks for replying
As per MTC of pipe, it's showing impact test at 0 degree C. Attached image for reference 

On Sun, 15 Jan 2023, 5:48 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Impact test shall be performed at -48degC

and pls ensure whether API 5L X60 is suitable for this temperature from the MTC

Thanks & Regards

J.Gerald Jayakumar




On Sunday, 15 January, 2023 at 02:36:04 pm GMT+3, Ritesh Kumar Singh <riteshsiwan770@gmail.com> wrote:


Dear expert's.

We are going to perform PQR  on material API 5L X60 (P1 G2 to P1 G2) 6" pipe.
Thk-21.95mm as per ASME sec 9.
Welding process-(GTAW Er70s-2(spl) + SMAW(E7018-1))


Client requirement are PWHT with impact test with other test as per code .
Kindly guide me for impact test temperature requirements.

We are qualifying this PQR  to weld rolled fittings of A537 CL1. thk 30 mm.
Design code ASME SEC 8 DIV1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-hPkO6LTuoUw2%2BdBnYR1P8ex-Ti9FMwk_OWUr6V681zpA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26135762.456028.1673784800697%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-j2b6NWVtzQ_XHrSQ6kzGi1QyMKM4D-iOXHse7EsgtveA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/624121096.911123.1673786247136%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/670180816.905141.1673787990390%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw9NbBOb4ueDJrrZkSb3JTSuh%2Bmq60UVxiDoC7zS4n%3Dsow%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1958138645.1041658.1673849418202%40mail.yahoo.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...