Skip to main content

[MW:33942] Re: SA387 GR.11 CL.2 Vessel

Manikandan,

1)Qualify PQR as per ASME SEC IX  . Additionally  consider and comply to  (API RP 934 C) with  BM as    SA 387 GR.11 CL.2 with butt joint /PWHT 
2)Qualify PQR as per ASME SEC IX  . Additionally  consider and comply to  (API RP 934 C) with  BM as    SA 387 GR.11 CL.2 with  WOL of TYP 347  /PWHT
   For WOL follow process which you want to use FCAW/GMAW/SMAW  

These two WPS s shall satisfy  your production Welding as mentioned  in above  query 

Thanks and regards

Vishwas -IWE 
International Welding Engineer 



On Thursday, January 19, 2023 at 4:38:56 PM UTC+5:30 manikandan J wrote:
Dear Experts,

We have a Vessel with the following MOC.(API RP 934 C)

Material 1 : SA 387 GR.11 CL.2 + SA 240 GR.347 (3.2 mm Cladded) -80 MM

Material 2 : SA 387 GR.11 CL.2 - 25 mm

Requesting your Technical inputs for PQR establishment.

Regards,
Manikandan
KSA

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/690c7c0c-7f90-4d67-ab86-96d8bf1043c1n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...